How It Works

Step 1

Send your file

STEP preferred, STL works too. Include the quantity and what the part does.

Step 2

We check it

Wall thickness, orientation, and anything to change for printability or fit.

Step 3

You get a quote

Based on the material and the machine time.

Step 4

We print it

In the engineering-grade material that suits the job.

Step 5

We finish it

Bores, threads and sealing faces machined where they need a precise fit.

Step 6

We ship it

Anywhere in the US.

Why Engineering-Grade Materials

Everyday printing plastics such as PLA soften at low temperatures and are not made for oils or chemicals. The materials we print are chosen for working parts: depending on the grade, they bring higher heat resistance, stiffness, toughness or chemical resistance. The comparison below shows how they differ.

How the Materials Compare

Indicative values only. These figures are typical values published by filament manufacturers, shown to compare materials in general terms. They are not guaranteed properties of any printed part and should not be used as design values. Real performance depends on the brand, print settings, part geometry and print orientation.

Swipe sideways to see the full table.

Material (strongest first)Tensile strengthStiffness (modulus)Heat resistance (HDT)Chemical and moisture resistanceExample usesWhy this material
1PPA-CFCarbon fiber reinforced polyphthalamide168 MPa
11.8 GPa
227 °Cat 0.45 MPa loadGood vs oils, fuels, greases and coolants. Absorbs less water than PA6.Engine-bay brackets, high-load arms, hot jigs and fixturesHighest strength and stiffness here, and it keeps them when hot. Trade-off: lower impact toughness.
2PA6-CFCarbon fiber reinforced nylon 6 (polyamide 6)102 MPa
4.4 GPa
164 °Cat 1.8 MPa loadGood vs oils, fuels and most solvents. Absorbs the most water of the group (about 2.4%).Gears, structural brackets, machine and automation partsStrong, tough and wear resistant. Best kept out of constantly wet service.
3PA612-CFCarbon fiber reinforced nylon 6/12 (polyamide 612)91.9 MPa
5.1 GPa
114 °Cat 1.8 MPa load (175 °C at 0.45 MPa)Good vs oils and fuels. Absorbs about 2.2% water at equilibrium.Outdoor and sporting gear, archery accessories, functional bracketsGood balance of strength, stiffness and toughness, and more forgiving than PPA-CF.
4PA12-CFCarbon fiber reinforced nylon 12 (polyamide 12)77.4 MPa
3.3 GPa
105 °CVery good vs oils, fuels and greases. Lowest water uptake of the nylons (about 1.5%).Fuel and oil line clips, housings, snap fitsTough and stable in humid or oily environments. Less stiff than the other nylons.
5PPS-CFCarbon fiber reinforced polyphenylene sulfide59.4 MPa
5.4 GPa
252 °Cat 0.45 MPa load, annealedExcellent. Resists most acids, bases and solvents. Almost no water uptake (about 0.2%). Flame retardant (UL94 V-0).Pump impellers and casings, chemical process parts, hot fluid manifoldsHandles heat and harsh chemicals at the same time. Trade-off: brittle, so not for impact loads.
6PETG-CFCarbon fiber reinforced polyethylene terephthalate glycol59 MPa
2.5 GPa
68 °CFair. Fine with water and many cleaners. Not for solvents or hot service.Jigs, fixtures, covers, indoor brackets, prototypesEconomical, accurate and clean looking. Good when heat and chemicals are not a concern.
7PPS-GFGlass fiber reinforced polyphenylene sulfide57.3 MPa
4.1 GPa
up to ~220 °Cat 1.8 MPa load, annealedExcellent, same as PPS-CF. Glass fiber makes it electrically insulating.Electrical housings and insulators, hot chemical servicePPS chemical and heat resistance where the part must not conduct electricity.
8PP-CFCarbon fiber reinforced polypropylene39.8 MPa
2.6 GPa
~70 °Cat 0.45 MPa loadExcellent vs acids, bases and many solvents. Almost no water uptake.Lab fixtures, tank fittings, fluid handling partsPolypropylene’s chemical resistance with much more stiffness than plain PP.
9PPPolypropylene~10 MPa
0.25 GPa
~64 °Cat 0.45 MPa loadExcellent vs acids, bases and cleaning chemicals.Living hinges, containers, chemical-contact partsFlexible and fatigue resistant. Bends without cracking, but low strength.

Ranked by tensile strength. All values are indicative only, taken from manufacturer data sheets for dry, printed test bars in the X-Y direction. Strength between layers (Z direction) is lower, and figures vary by brand, print settings and part design. Heat resistance is the heat deflection temperature (HDT): the temperature at which a test bar starts to bend under a set load. A lighter load gives a higher number, so the test load is shown under each value where the data sheet states it. Annealed means the part was heat treated after printing. PP and PP-CF stiffness is flexural modulus. Not sure which material fits your part? Tell us about the load, temperature and chemicals it will see and we will recommend one.

Good Fits for This Service

Jigs and fixtures

Holding, locating and assembly tooling.

Brackets and mounts

Including housings and covers.

Functional prototypes

Test the fit and function before committing.

Small batches

End-use parts with no minimum order.

Fluid handling

Chemical and fluid-contact parts.

Replacement parts

Remade from your file or the old part.

No tooling cost. Design tip: keep walls at least 1.2 mm thick.